Typical Short Time Tensile Properties as a Function of Temperature
Typical room temperature tensile properties of material annealed at 1920°F (1065°C) follow.
| Temperature | 0.2% Yield Strength | Ultimate Tensile Strength | Elongation Percent | |||
|---|---|---|---|---|---|---|
| °F | °C | psi | MPa | psi | MPa | |
| 1920 | 1065 | 63,000 | 430 | 136,000 | 940 | 51.5 |
Data shown are typical, and should not be construed as maximum or minimum values for specification or for final design. Data on any particular piece of material may vary from those shown herein.